Specification:
Broad transparency range from 160nm to 2600nm
High optical homogeneity (dn?10-6/cm) and being free of inclusion
Relatively large effective SHG coefficient (about three times that of KDP)
High damage threshold (18.9 GW/cm2 for a 1.3ns laser at 1053nm)
Wide acceptance angle and small walk-off
Type I and Type II non-critical phase matching (NCPM) in a wide wavelength range
Spectral NCPM near 1300nm
Application:
Optical parametric amplifiers(OPA) and oscillators(OPO);
Frequency doubling(SHG) and tripling(THG)
Diode laser pumped Nd:YAG and Nd: YLF laser. Alexandrite, Ti:Sapphire, Dye Lasers, Ultrashort Pulse Lasers
Dimension tolerance: (W 0.1mm) x (H 0.1mm) x (L + 0.2mm/-0.1mm)
Flatness: λ/8 @ 633nm
Scratch/Dig code: 10/5 Scracth/dig per MIL-O-13830A
Parallelism: better than 10 arc seconds
Perpendicularity: 5 arc minutes
Wavefront distortion: less than λ/8 @ 633nm
Clear aperture: > 90% central area
Coating: AR/AR: 1064nm / 532nm R1064<0.1% R532<0.2%
AR/AR: 532nm / 266nm R532<0.2% R266<0.5%
AR/AR: 1064nm / 355nm R1064<0.2% R355<0.5%